See all updates by Joseph Fireborn
-
Testing a new glaze firing schedule. Trying to rid myself of microdimples when working with good ole GB.
-
try doing a hold on the cooling at 1900 for 30 minutes.. it may give the glaze more time to smooth out ..
-
I did a hold at 2115 for 45 minutes. Helped a lot. Still not as smooth as I want though. But definitely improved. I am thinking about doing several holds on the way down. Going to keep testing cause the glaze surface definitely looks way better than before.