I will conquer this black clay bloating problem if its the last thing I do on this earth!
- Show previous comments 5 more
-
Seattle Pottery claims their vashon series goes to ^6, as well as their crystal white porcelain. All of those bodies bloat like a gassed-up politician. Sooooo...either the clay's being over-fired, or your kiln might be a bit too hot.
-
Maybe, but others have stated they have fired to cone 6. I use self supporting witness cones. I am not over firing, if anything under firing. I go to about 5.5.
-
Good luck I have no idea about bloating.