Picked up my compressor and sprayers today. Going to hook it all up tomorrow and start practicing. Really excited about the ability to control my glaze application a lot more than dipping and brushing.
- Show previous comments 3 more
-
Spray is nice but a slower process
-
I don't mind the slower process if I get the results I want. I will still dip and pour a lot of things but there are things I want to spray like large bowls that I can't dip without huge amounts of glaze, and I have tried pouring them to very unsuccessful results.
-
I still have a tendency to start with dip/poured base and add accents with spray and hand brushing.