This may be your manual https://skutt.com/images/KilnSitterManualOldPre1980.pdf Note the section on Testing Models 181 & 145 on p2.
-
SDS at https://tinyurl.com/2csusk8r Mentions: Silicon dioxide Calcium carbonate and dolomite Nepheline Syenite Rutile Zinc oxide ... all max 15%
-
I did a search for "Split LOI" in "Content tiles and body" covering "everywhere" and only got hits for two of your postings in this thread. ... and another for glazenerd postings in 2019 mentioning LOI (it insisted on a some text to match) again without success. ... a search for anything by PeterH posted in 2019 and containing "the" also failed. ... looks like none of my posts before 2022 are there. @Hulk How long are posts kept? Are there any non-active backups about? BINGO a google search for "Split LOI" test found So either my searches were NBG or the search function doesn't search all postings.
-
https://www.dickblick.com/products/blick-stoneware-clay/ Bisque fire to Cone 04 (1971°F, 1077°C). The firing range is Cone 5–10 (2205°F–2381°F). When fired at the recommended temperature of Cone 5 (2205°F), the hard, dense, semi-vitreous ware is creamy tan color with a shrinkage of 12% and absorption of 1.8%. At Cone 10 (2381°F), the very dense, vitreous ware is a soft gray color with a shrinkage of 13.2% and absorption of 0%.
-
Potentially relevant?
-
Another "bought an old kiln help me thread" :)
PeterH replied to Skydve76's topic in Equipment Use and Repair
As I said don't take my word for it, but I think that's what the gurus will say. I'm just giving a rationale based on my opinion. -
Another "bought an old kiln help me thread" :)
PeterH replied to Skydve76's topic in Equipment Use and Repair
Take the gurus advice on what to do about the wiring/breaker. But, if their response is what I expect, this is my understanding of why. >On the silver panel it says 30 amps. On the sitter it says 45 amps. I think you will find that this means - the kiln pulls up to 30a - the sitter can control a kiln pulling up to 45a So the load your circuit breaker will need to handle is 30a. But when supplying continuous loads circuit breakers may trip before their rated load. Information Sheet # 37 Differences Between 80% and 100% Rated Circuit Breakers https://cliffordpower.com/wp-content/uploads/2020/01/IS_37_80-versus-100-rated-ATS.pdf Typical circuit breakers are rated at 80%, so you would need a breaker and wiring rated at 30x1.25=37.5a, i.e. a 40a one. > I read on this forum a 60A circuit may be needed which is INSANE. I HIGHLY doubt that gray 10-50 plug is rated for 50A if that. You need an appropriately sized fuse in the plug to protect the kiln and its lead/plug/socket. The breaker prevents the house wiring from overheating (fire risk): hence the house wiring needs to be rated at the full breaker current, not the expected load. -
Large quantities of wild clay(water processing very slow)
PeterH replied to TunnleBricks's topic in Clay and Glaze Chemistry
+1 Would a local historical society know about such buildings in your locality? It's where we found out about some of the older/more-unusual buildings in my area (Essex). Just the 1st background reading I found, so no claims about its quality. How to make mud bricks, and why you might want to https://www.heifer.org/blog/how-to-make-mud-bricks-and-why-you-might-want-to.html Mud brick https://www.yourhome.gov.au/materials/mud-brick ... note the mention of cement-stabilised soil bricks -
IMHO the problems of thermal shock make this a highly "challenging" project. Not least because you will presumably be "guaranteeing" your customers that is safe to put these vases on top of their cherished woodwork. However a couple of observations. What sort of raku finishes were you thinking of using? Presumably the "crackle" ones demand a certain amount of thermal shock to start the crackle before smoking, while any thermal shock involve in "reduction" is incidental and not necessary for the final effect. Indeed thermal shock of reduction pieces might be minimised by firing them in an (open-topped?) saggar, which could be taken out of the kiln and reduction materials added to the saggar. OTOH the crackle finishes might stand up better the the ware-and-tear (and wetting) a vase is subject to. I assume a liner glaze on the inside of a pot would be less subject to thermal shock than the outside of the pot. I'll just mention an oddity that the raku artist Tim Andrews produced. The glaze was a mid-fire crackle, which he fired and cooled as normal. He then re-fired/warmed the pot before taking it from the kiln and covering it with sawdust. Minimising the 2nd firing temperature, and presumably thermal shock, involved in smoking the already crackled pot.
-
Large quantities of wild clay(water processing very slow)
PeterH replied to TunnleBricks's topic in Clay and Glaze Chemistry
My uncle built his own house, so I'm fully aware that it's doable. However have you checked to see if the use of home-made bricks might interact with such things as: - Planning and building regulations. - House insurance. - Resale; e.g. is there any impact on the buyer obtaining a mortgage. -
Large quantities of wild clay(water processing very slow)
PeterH replied to TunnleBricks's topic in Clay and Glaze Chemistry
Appendix 3 of Michael Cardew's Pioneer Potter contains a few pages on brick making with minimal facilities. Apparently simple bricks are made by slop-moulding using the sort of open frame Callie mentioned, although multi-brick moulds can speed things up. He suggests the slower stock-molding is used for special bricks (end-arches, side-arches,springers, bull-noses, flats, etc). The bricks are fired in a clamp, and the outer layer(s) of bricks are apparently discarded after firing. 45,000 bricks give a clamp about 30ft long, 15ft wide and 12ft high - with about 5,000 (12%) of the bricks discarded. 4,000-5,000 bricks gives a clamp about 10ft by 10ft by 8ft6in - with about 40% of the bricks discarded. He discusses a clamp for about 25,000 bricks with 10 fireplaces, and suggests that at least three-quarters of a cord of wood per 1,000 bricks are needed. It seems with care you can fire for 48hrs before you need to draw the embers. The firing is apparently finished when the top course of bricks glows red. I've no idea how long a total firing takes. PS IIRC elsewhere he discusses a bootstrap process if you want to use the bricks to make a kiln. First make a "sacrificial" kiln of clamp-fired bricks, and then fire another load of bricks in this kiln to a higher temperature for use in "real" kiln-building. (Assuming your cay is suitable.) -
Old thread ...
-
Slightly larger/more-legible version of the wiring diagram at https://skutt.com/images/181-Wiring-Diagram.pdf
-
HELP! Severe Shivering White Glaze
PeterH replied to clayenthusiast's topic in Clay and Glaze Chemistry
No comment on the "quality" of the glaze, just the numbers. Looks like a fairly direct conversion of Coleman No Craze White https://glazy.org/recipes/3331 Custer for G-200, kaolin for EPK and silica slightly changed ... with the addition of bentonite and zircopax. The original recipe added up to 970 rather than 1000, which might account for funny numbers. PS Glazy seems to have the same recipe listed under Coleman No Craze White (New Zealand Halloysite) https://glazy.org/recipes/3806 ... which claims to be Adjusted for New Zealand Halloysite. -
Have you thought about adding table salt? (Quick clay is formed by leaching sodium from the original marine clay.) ... although I believe that potassium chloride is now used for quick-clay landslide mitigation https://tspace.library.utoronto.ca/bitstream/1807/124221/1/cgj-2021-0230.pdf
-
Looks an interesting topic. Quick clay https://en.wikipedia.org/wiki/Quick_clay ... high-sodium marine clay changes is characteristics after the sodium is leached out. Quick clay landslides: an online documentary about Rissa https://blogs.agu.org/landslideblog/2020/06/18/rissa-ngi-video/ ... showing stiff-ish "found" clay liquefying under pressure to a pourable consistency. After adding salt it it is stiff enough to hold a knife upright. Quick though: are you looking at the properties of the as-dug clay, or has the washing involved in the filtering removed even more sodium? PS If you can give us the location where you found the clay perhaps somebody can find it on a geological map.
-
Stoneware Slip questions (UK potter)
PeterH replied to BristolPotter's topic in Mold Making and Slip Casting
>Yes, I'm buying in the powdered clay from Potclays, it's their 1145. I have been using way more sodium silicate (based on the recipe for casting slip from Potclays themselves), so I suspect earthenware might behave quite different to stoneware I'm a little confused. Looking at Potclay's site they seem to give a "starting point range" rather than an actual recipe. Can you confirm this is what you are trying to use? https://www.potclays.co.uk/clays-slips-grogs/clays-slips-grogs-powdered-clays/white-st-and-39;ware-powder https://www.potclays.co.uk/recipe-casting-slip-powdered-clay As you don't have a definitive recipe I assume that you are doing small-scale experiments until you work one out. I assume that you started by exploring the range of recipes in Potclays recipe-range. Perhaps by a some variation on "keep slowly adding deflocculant until you reach the sweet spot" (or more precisely until you've overshot it a bit, but can reconstruct the recipe at the sweet spot). A rather formal version of the process is given in Determining Dispersant Additions for Casting Slips https://static1.squarespace.com/static/527ac372e4b0d4e47bb0e554/t/527fd7f1e4b0c046bfa9b90d/1384110065234/Dispersant+Addition+Procedures.pdf My guestimate based on Brongniart's formula suggest that these slips would have a SG of about 1.75 to 1.78 (see PS). So if the slip at the sweet-spot had been acceptable it would probably have met your needs. How bad was it? If the slip at the sweet-spot wasn't acceptable it might be worthwhile asking Potclays how you should proceed, as it makes their advice look potentially suspect. >Yea they are saying to use 3.5g for every 1000g of dry material but I haven't found that to get anywhere near fluid enough and I am using double that at 7g for every 1000g of dry material. But it's Potclays recipe advice for their clay. If their advice has any validity surely this should be resulting in significant overflocculation. Either something is badly amiss or Potclays recipe is totally misconceived. BTW can you confirm that your sodium silicate is 120tw and your soda ash is fresh. PS I note that Potclays recommend 25kg clay in 10l of water. So I'll try to work out its SG. Based on http://www.potteryatoldtoolijooaschool.com/brongniarts_formula_made_easy.pdf SG of clay is 2.5 to 2.6 And making Brongniart's assumption that the solids don't dissolve, but simply occupy their volume in the final slip ... Weight of slip = weight-of-clay + weight-of-water = 25kg + 10kg = 35kg Volume of slip = volume of clay + volume-of-water ... between 10 + 25/2.6 and 10 + 25/2.5 litres = 19.6 to 20 So SG of Potclay's slip is weight/volume = 1.75 to 1.78 -
A thread with a few references An online book 21st Century Kilns, and a few articles http://www.clayartarchives.com/
-
https://www.bookfinder.com/ is a good source for harder-to-find books. When you get to the list of matching books I find the or view all matches combined option useful.
-
A hybrid technology: stainless steel ring with inlay (here polymer clay). Video using Fimo Soft (maybe not the best polymer for jewellery) One source for suitable stainless steel "inlay" rings https://www.amazon.co.uk/dp/B09N6XQ1LG/ref=twister_B091KYY4B1?_encoding=UTF8&psc=1 PS This may be relevant Best Polymer Clay for Earrings and Jewellery https://sarahmaker.com/best-polymer-clay-for-earrings-and-jewelry/
- 17 replies
-
Sort of, but ... - The SG of water varies with temperature. - Dissolved solids will increase the SG (mainly thinking of hard water). Size of the effects on SG seem small enough to ignore "for government work" https://www.hillcrestplumbingandheating.com/b/hard-water-vs-soft-water-debate-finally-solved The Guidelines for Canadian Drinking Water Quality Hardness rank hard to soft by CaCO3 levels. Here are their guidelines: Soft Less than 60 mg/L Medium Hard 60 to 119 mg/L Hard 120 to 179 mg/L Very Hard 180 mg/L or greater
-
Can you confirm that you are using CMC, not the Ceradel label gum.