Just turned on a bisque load- this one contains little handprints on slabs for my sons preschool class, they are my first slabs and have already warped a lot, but I need to get them done before school lets out this year.
- Show previous comments 5 more
-
For slabs dry them for several days between two pieces of dry wall,moving to drier place frequently.
-
Ben- Probably the humidity. The thickest part was maybe 1/3 of an inch. Rakujane- thanks for the idea. I know nothing about working with slabs!
-
Rebekah, did you do any candling, or slow fire around 200 F or 900 F?