branch vase
This vase is about 6 square. I threw it then carved grooves in the top and bottom. The grooved sections get a couple coats of black engobe because I like the way the glaze looks over the black. The middle is black engobe with paper branches then blue engobe then the paper is peeled off. It has commercial glazes and was fired to cone 6 in my electric kiln. I tried to get fancy with the picture.