Posted 14 June 2013 - 11:14 AM

Ok having only used commercial glaze, I would love to try mixing one on my own. Does anyone have a recipe for a pretty light peach / melon color? Cone 5-6 As simple as possible?
Learning On my Kick wheel with my vintage Paragon (from the late 1960's)

#2 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 1,975 posts
  • LocationCentral, PA

Posted 14 June 2013 - 11:20 AM

Ok having only used commercial glaze, I would love to try mixing one on my own. Does anyone have a recipe for a pretty light peach / melon color? Cone 5-6 As simple as possible?


Alas, you have run into a range of color that is a little more difficult without the use of a stain. Most orange and red colors as your melon is between the two are more difficult at ^6. So I would start with a base opaque, and add a Mason stain. Others might have a recipe that depends on the interaction of chromium and tin, but I don't have one for that color.

Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . .                                                                                 http://picworkspottery.blogspot.com/


#3 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 835 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 14 June 2013 - 01:38 PM

yes, contact me by email with more details. i have several with varying shades of peachiness with simple base recipies and a little stain.
"putting you down does not raise me up."

#4 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 14 June 2013 - 02:07 PM

This recipe is a ripe cantaloupe color.

EPK14.00g Silica26.00g Wollastonite14.50g F-4 Feldspar24.00g Frit 324920.00g

Add 5% of Mason stain 6121

Good Luck!
Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#5 Gary Taylor

Gary Taylor

    Newbie

  • Members
  • Pip
  • 8 posts

Posted 14 June 2013 - 03:23 PM

Darrel

I can't wait to try your ripe cantaloupe glaze but a little confused with the Frit. Is that 20 grams of Frit 3249? My eye sight isn't great and I can't quite make it out.
Sorry if that's a dumb question.

Thanks

Gary Taylor

#6 Wyndham

Wyndham

    Advanced Member

  • Members
  • PipPipPip
  • 389 posts
  • LocationSeagrove NC

Posted 14 June 2013 - 08:14 PM

Gary, looks like 20 grams is what Darrel was saying. Looks like an interesting glaze. if you like the look of the finish, which looks like it should be a gloss, you could use this as a base glaze and use other stains to get a wider pallet of glaze colors.
Wyndham

#7 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 15 June 2013 - 12:39 AM

Darrel

I can't wait to try your ripe cantaloupe glaze but a little confused with the Frit. Is that 20 grams of Frit 3249? My eye sight isn't great and I can't quite make it out.
Sorry if that's a dumb question.

Thanks

Gary Taylor


Yes, 20 grams of frit 3249
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#8 Rebekah Krieger

Rebekah Krieger

    Advanced Member

  • Members
  • PipPipPip
  • 508 posts
  • LocationWisconsin

Posted 17 June 2013 - 02:11 PM

Thank you so much for the help! I Will gather supplies for my first mix and make an attempt at this :)
Learning On my Kick wheel with my vintage Paragon (from the late 1960's)

#9 Min

Min

    Advanced Member

  • Members
  • PipPipPip
  • 429 posts
  • LocationCanada

Posted 17 June 2013 - 03:06 PM

The clear base glaze that Darrel posted, G1215U, is a wonderful clear for low expansion clays. It's expansion is 5.71 so it's probably going to shiver on a lot of clays. Min

#10 Gary Taylor

Gary Taylor

    Newbie

  • Members
  • Pip
  • 8 posts

Posted 17 June 2013 - 03:47 PM

Thank you for the clarification of the frit and weight.

Gary Taylor