What are your tricks to make unglazed bottoms of stoneware items less abrasive? I don't want them to scratch table or countertop surfaces.

Do you polish them with diamond wheels/points or belt sanders? Any other approaches short of attaching felt?


Thank you.

#2 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,672 posts
  • LocationNorthern Virginia

Posted 23 March 2013 - 06:59 PM

I use 3-M diamond polishing pads that I get from toolocity. 50/100/200 grit. Wet sand . . . dunk the pad in water, sand/polish. Doesn't take much time, but it makes a world of difference.

http://www.toolocity...shing-pads.aspx

#3 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 23 March 2013 - 08:34 PM

I sand all of my work. I first sand with a green "stainless steel wool" type thing for kitchen scrubbing.After glaze firing I sand bottoms with course sandpaper. Wear a dust mask.
TJR.

#4 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,128 posts
  • LocationWilton, NH USA

Posted 23 March 2013 - 09:25 PM

Slow revolution wet silicon carbide grinder with a wide wheel. Diamond blade for the first go on the really nasty stuff (I'm a woodfirer).

best,

......................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#5 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,079 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 24 March 2013 - 12:26 PM

Back when I did stoneware I ran them all on a 6 or 8 inch brass wire wheel mounted on the bench grinder. Really did a good job fast.
Mark
Mark Cortright
www.liscomhillpottery.com

#6 MichaelP

MichaelP

    Advanced Member

  • Members
  • PipPipPip
  • 190 posts
  • LocationIL/WI border

Posted 24 March 2013 - 05:14 PM

Thank you for sharing your techinics!

#7 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 2,977 posts
  • LocationCentral, PA

Posted 24 March 2013 - 07:01 PM

What are your tricks to make unglazed bottoms of stoneware items less abrasive? I don't want them to scratch table or countertop surfaces.

Do you polish them with diamond wheels/points or belt sanders? Any other approaches short of attaching felt?


Thank you.


I use silicone carbide sandpaper adhered to a bat on the wheel. Works well for the fines stuff. For bigger stuff a dremel. Always a mask!
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#8 MichaelP

MichaelP

    Advanced Member

  • Members
  • PipPipPip
  • 190 posts
  • LocationIL/WI border

Posted 24 March 2013 - 08:05 PM

I use silicone carbide sandpaper adhered to a bat on the wheel.

This is an excellent idea!

#9 Bette

Bette

    Advanced Member

  • Members
  • PipPipPip
  • 32 posts
  • LocationMorgan Hill, California

Posted 24 March 2013 - 09:57 PM

Baileys carries a silicon carbide disk that with adhesive backing - fits on a standard bat so you can use your wheel

#10 timbo_heff

timbo_heff

    Advanced Member

  • Members
  • PipPipPip
  • 205 posts
  • LocationMA / NY

Posted 25 March 2013 - 08:31 AM

I have taken to burnishing the foot more when leather hard ... saves on dusty, loud post-firing finishing. Then a tiny hit with waterproof sandpaper finishes the foot very quickly with no dust.