I'd like to hear some compelling reasons for using a sieve for making glazes.

#2 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 13 October 2012 - 04:41 AM

Lumps.
Maryjane Carlson

Whistling Fish Pottery

#3 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,810 posts
  • LocationGrayslake, IL

Posted 13 October 2012 - 08:50 AM

Gets out the lumps. A mixer won't cut it, unless you have a high shear industrial mixer....

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com


#4 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,124 posts
  • LocationWilton, NH USA

Posted 13 October 2012 - 09:32 AM

Most compelling is that if you want your glazes (typically) to look good, seiving assures that. Consistency.

best,

.......................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#5 Nelly

Nelly

    Advanced Member

  • Members
  • PipPipPip
  • 380 posts

Posted 13 October 2012 - 02:53 PM

Most compelling is that if you want your glazes (typically) to look good, seiving assures that. Consistency.

best,

.......................john



Dear All,

I totally agree with all that has been said. Grit. Lumps that somehow get into the glaze and you don't notice them until they are smack gob on the middle of your pot after firing. When at all possible I like to seive before I dip or pour. Then I gently review the piece looking for little air bubbles. I smooth these out as well. Any cracks in the glaze from big gobs I scrape off and start again.

And I think the taliman seive is a great invention. I recall the days we painted glazed through seives with brush. It was hard work. If you don't have one a talisman is great for the initial mixing. I used the wire strainers you can get from the dollar store when it comes to seiving smaller amounts.

Nelly

#6 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,124 posts
  • LocationWilton, NH USA

Posted 13 October 2012 - 03:59 PM

And I think the taliman seive is a great invention.



+1

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#7 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,131 posts
  • LocationRed Lodge, Montana

Posted 14 October 2012 - 12:28 AM

yep. lumps. Ugly white ones. I was a guest artist at a center recently and used the center's glaze as part of prepping for a firing demo. it was not sieved. Got awful lumps on a very large bowl.
I tried refiring it when I got home but you can't cover up those lumps.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#8 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 14 October 2012 - 09:17 AM

Not just lumps, but general distribution of ingredients. You can get streakiness, blotchiness, color variation... or even faults like crawling in some cases.

I once skipped the sieve step with a glaze that was heavy on the copper oxide (just wielded the mixer like madman). It looked OK in the bucket, but gave the most oddball, variegated effects I'd ever seem. Not even displeasing... but totally unpredictable.
Not all who wander are lost

#9 Denice

Denice

    Advanced Member

  • Members
  • PipPipPip
  • 1,214 posts
  • LocationWichita, Kansas

Posted 14 October 2012 - 10:53 AM

Can''t imagine making glazes without sieves, I have a small one for test glazes and a bowl type for larger batches. The larger one is about 30 year old and is starting to wear out I keep patching it with silicone. I'm turning 60 Monday so I think I'm going to treat myself and order a talisman. Denice

#10 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,124 posts
  • LocationWilton, NH USA

Posted 14 October 2012 - 11:58 AM

I'm turning 60 Monday so I think I'm going to treat myself and order a talisman.


Happy Birthday, Denise.

And you won't go wrong wit hthe Tallisman seive. Altjough I wish they still made the body of aluminum (I have one of each).

best,

..............john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#11 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 14 October 2012 - 05:58 PM

I sieve all of my glazes every time I go to glaze. I sieve first through an 80 mesh sieve, wash the 5 gallon bucket, then sieve the glaze back into the original bucket through a 100 mesh sieve.
If you don't sieve, you have lumps and inconsistency of texture.
Go buy a sieve.I can't believe I used the word sieve eight times.
TJR.

#12 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 14 October 2012 - 05:58 PM

I sieve all of my glazes every time I go to glaze. I sieve first through an 80 mesh sieve, wash the 5 gallon bucket, then sieve the glaze back into the original bucket through a 100 mesh sieve.
If you don't sieve, you have lumps and inconsistency of texture.
Go buy a sieve.I can't believe I used the word sieve eight times.
TJR.

#13 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,668 posts
  • LocationNorthern Virginia

Posted 14 October 2012 - 07:42 PM

As I was mixing a new batch of slip this afternoon and using a scrub brush to work the slip through a 60 mesh sieve, this discussion of the benefits of a Talisman kept ringing in my mind.

#14 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,079 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 15 October 2012 - 07:49 PM

Talisman 80 mesh for me-everything goes thru it and all is well afterwards.
I have all the screen sizes but long ago found the 80 to be enough for 99.9% of needs-now after wearing out 3 of them its still true.
The big labor savers are when clay is your livelihood
pre made clay
power wheel
Talisman sieve
Power mixer for glazes
car kiln
electric slab roller
I wish I had them all when I was younger-or at least my body does.
Mark
Mark Cortright
www.liscomhillpottery.com

#15 Idaho Potter

Idaho Potter

    Learning all the time

  • Members
  • PipPipPip
  • 403 posts
  • LocationBoise, Idaho

Posted 16 October 2012 - 07:00 PM

If a glaze hasn't been used in awhile, it should be sieved before using because ingredients tend to clump and lump if left undisturbed. I was laughed at for sieving my raku glazes ( I guess because so many of them are made using borax) but running the glaze through a screen mixes everything well, and if there are small particles (usually crystalline) I use the last of the mixing water to rinse them back into the mix, so I lose nothing.