Kaolinwasher Posted July 1, 2017 Report Share Posted July 1, 2017 this is from my last firing, cone 8 reduction, needed just a bit more heat but turned out good . This is my anoka sand Celadon glaze, and porcealin both made with the anoka sand i use 56% anoka sand in the body and glaze, the anoka sand is an arkose sand having about 25% feldspar in it the iron deoration around the rim is diabase basalt 100% Link to comment Share on other sites More sharing options...
yappystudent Posted July 1, 2017 Report Share Posted July 1, 2017 Alchemical wizardry. Link to comment Share on other sites More sharing options...
Judith B Posted July 1, 2017 Report Share Posted July 1, 2017 you used a different glaze on the rim? I love the effect! Link to comment Share on other sites More sharing options...
Joseph Fireborn Posted July 2, 2017 Report Share Posted July 2, 2017 The celadon itself is very nice. The running effects also add to the pot to make it not just another celadon bowl. Nice work good sir. I really like it. The best part is all the natural stuff you found. Really makes it more personal and awesome. Link to comment Share on other sites More sharing options...
oldlady Posted July 2, 2017 Report Share Posted July 2, 2017 and the bowl is not so bad either! good job! Link to comment Share on other sites More sharing options...
Kaolinwasher Posted July 6, 2017 Author Report Share Posted July 6, 2017 ready to make another one . but a rabbit almost ruined it . It had dug under the shelter and knoked over the bricks that cover the burner port . if a mouse got in that could be a badd thing Link to comment Share on other sites More sharing options...
Marcia Selsor Posted July 6, 2017 Report Share Posted July 6, 2017 really lovely color of celedon marcia Link to comment Share on other sites More sharing options...