nancylee Posted February 17, 2016 Report Share Posted February 17, 2016 Hi all, I used this a few years ago and can't find my notes. (What else is new?) I know/think it was a low fire paint on glaze, but I'm not sure. Anyone recognize this? Thanks in advance for any help, Nancy Link to comment Share on other sites More sharing options...
Cavy Fire Studios Posted February 18, 2016 Report Share Posted February 18, 2016 Hmmm, I'm a die-hard lowfirer, but have never seen that. Maybe Benzine knows? Link to comment Share on other sites More sharing options...
LeeU Posted February 18, 2016 Report Share Posted February 18, 2016 Could it be a mix of several different (same cone) glazes? I have done pieces intended to come out similar to the cup pictured, using 3-4 commercial glazes. Link to comment Share on other sites More sharing options...
nancylee Posted February 19, 2016 Author Report Share Posted February 19, 2016 Could it be a mix of several different (same cone) glazes? I have done pieces intended to come out similar to the cup pictured, using 3-4 commercial glazes. Hi,No, I know it's just one glaze. I was playing with some funky glazes for a while, ones with starburst, etc. I think it's one of those, but can't remember which one. Thanks! Nancy Link to comment Share on other sites More sharing options...
Benzine Posted February 19, 2016 Report Share Posted February 19, 2016 Hmmm, I'm a die-hard lowfirer, but have never seen that. Maybe Benzine knows? Sorry, I'm at a loss too. It's not one I've ever used. If I were trying to replicate that, I'd be layering a couple glazes, like others have suggested. Link to comment Share on other sites More sharing options...
perkolator Posted February 19, 2016 Report Share Posted February 19, 2016 Are you looking for a commercial glaze or a recipe for a glaze that will do that effect? Link to comment Share on other sites More sharing options...
bciskepottery Posted February 19, 2016 Report Share Posted February 19, 2016 It appears (at least to me) that the glaze has crawled substantially. Link to comment Share on other sites More sharing options...
Min Posted February 19, 2016 Report Share Posted February 19, 2016 just a wild guess but if was just one glaze then maybe one of these? looks overfired maybe? http://www.bigceramicstore.com/duncan-crystals-crackles-14770.html http://www.amaco.com/products/glaze-ctl-9-snap-dragon?taxon_id=277 Link to comment Share on other sites More sharing options...
nancylee Posted February 20, 2016 Author Report Share Posted February 20, 2016 I'm looking got a commercial glaze. I think it might be one of those shown, Thank you, Nancy Link to comment Share on other sites More sharing options...
nancylee Posted April 17, 2016 Author Report Share Posted April 17, 2016 Thought I'd bump this since someone saw it somewhere on line and is interested in it. I think it's a commercial,"flow" glaze, but I still can't find the color online. Thanks, Nancy Link to comment Share on other sites More sharing options...