Joe_L
-
Posts
183 -
Joined
-
Last visited
Reputation Activity
-
Joe_L got a reaction from Pyewackette for a gallery image, IMG 1966
9cm Stoneware Single Fired Cone 9 - Cobalt slip
-
Joe_L got a reaction from Pyewackette for a gallery image, IMG 1967
8cm Stoneware Single Fired Cone 9 - Cobalt slip
-
Joe_L got a reaction from Pyewackette for a gallery image, IMG 1995
11cm Stoneware Single Fired Cone 9
-
Joe_L got a reaction from Pyewackette for a gallery image, IMG 1943
13x16cm Oval. Thrown and altered. Wood fired, Cone 10 reduction.
-
-
Joe_L got a reaction from Pyewackette for a gallery image, Experiment with glazes running and interacting
ES10 Stoneware Cone 9 (electric)
-
-
-
-
Joe_L got a reaction from Mark_H for a gallery image, Experiments with glaze interaction and flow
Stoneware, single fired to Cone 9 (electric)
-
-
-
-
-
-
Joe_L reacted to Linda Lees for a gallery image, IMG_8096.JPG
Slab construction, stoneware with a crackle celadon glaze.
-
-
-
Joe_L reacted to ZAN Ceramics for a gallery image, Moss Pebble Vase Collection
Moss Pebble Vase Collection
-
Joe_L reacted to firenflux for a gallery image, Big circles vase (1)
This is my favorite piece I have made to date. I sold it about a year ago but haven't made another one yet. It's wheel thrown with applied colored engobes. It's hand carved and textured with pulled handles and commercial glazes. Fired to ^6 electric.
-
Joe_L reacted to firenflux for a gallery image, Green geometric cup
I love all the varied shapes a good mug comes in. The shape is my current favorite. It works well to separate the textured areas from the geometric sgraffito in the bottom. It has a pulled handle and commercial glazes and was fired to cone 6 electric.
-
Joe_L got a reaction from glazenerd for a gallery image, Experiments with glaze interaction and flow
Stoneware, single fired to Cone 9 (electric)
-
-
-
-
-
-
-
-