Bowl for my throwing water, complete with grooved flat area for holding tools and sharp rim for wiping slip off hands.

Wood-fired Cone10 Reduction, Tenmoku glaze.

From the album:

More Bowls

  • 6 images
  • 0 comments
  • 1 image comment

Photo Information for IMG 1952

Taken with Canon Canon DIGITAL IXUS 70

  • 12.1 mm
  • 1/800
  • f f/4.0
  • ISO 80
View all photo EXIF information
 Share


Recommended Comments

I love the look of leaving part of the pot unglazed! I just ordered in a low porosity red clay and threw some test pots to give this look a go. Really like the red clay but hate getting every speck of it cleaned up after. (I use white clay)

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.