Hi,

I'm planning to make  a sculpture that is about 29 inches high and 15 inches wide, it will be wheel thrown so imagine a tall cylinder... it has a really delicate heavy texture on the exterior of the piece so I am wondering what I should build on so that when I move it to the kiln I wont need to actually grab it with my hands and risk messing the texture up. I will be firing in an skutt electric that I can disassemble. A few thoughts - I have heard of people firing on drywall, is this ok for the elements? What about just building on top of a kiln shelf? I plan on putting sand underneath what I build. Any advice would be appreciated. 

Thank you!

Edited by tman123
Link to comment
Share on other sites

13 minutes ago, tman123 said:

I have heard of people firing on drywall, is this ok for the elements? What about just building on top of a kiln shelf?

Don’t fire on drywall it will smolder and burn once calcined. Used to be type X 5/8” - approx. 60 minutes, 120 minutes to sustain a flame. I like the shelf idea and unless once firing, you can grog / silica the shelf after bisque. Many of our large format sculptors would build on a very straight shelf on top of a four wheeled cart.

Link to comment
Share on other sites

Build it on a shelf. I think that’s a great idea. Taking rings off the Skutt is a solution to the next problem, you’re thinking it through (You really need a car kiln or front loader for this!). Wheeled carts are brilliant.

I struggle with this next bit, because I would rather do things on my own and screw them up (It’s a blessing and a curse) than have either help or an audience. This is a large piece. Having another pair of trusted eyes and hands is indispensable, enlist help for the critical move if you haven’t already considered it. 

Link to comment
Share on other sites

Definitely build it right on a kiln shelf. I'd also put it on a waster slab. It's okay if the waster breaks, it'll still work. Keep the kiln shelf up on bricks or something that will allow you to get your fingers under the edge to pick it up without having to tip it.

Link to comment
Share on other sites

  • 2 weeks later...

I have fired many large pots and sculptures that filled the kiln.  Taking the kiln apart and candling over night is the way to go,   I also use a shelf to  build  and fire it on,  I pick one that is not in the greatest shape.  I am getting ready to work on new sculpture,  I have already figured out a way to make it in two pieces so I don't have to take my new kiln apart.    It only has 16 firings on it and it is bigger around than my old skutt but shorter.    The rings are harder to manage,  I am not ready to bump, scuff and chip the edges yet.   Denice

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.