Shaina Mahler Posted November 26, 2023 Report Share Posted November 26, 2023 Hi everyone, Does anyone know how to achieve this look, specifically the white glaze? These pictures might all show different techniques/types of glazes, but I’d appreciate insight on any of them. I’m guessing these examples weren’t done with commercial glazes. Thank you for any advice Quote Link to comment Share on other sites More sharing options...
Morgan Posted November 27, 2023 Report Share Posted November 27, 2023 Super hard for me to see the pics are small to my eyes but looks like it could just me as simple as brushing on a white matte glaze unevenly/thin/thick and maybe a brushed cobalt wash? Could be underglaze but seems more like a wash from afar. Rae Reich, PeterH and Roberta12 3 Quote Link to comment Share on other sites More sharing options...
PeterH Posted November 27, 2023 Report Share Posted November 27, 2023 (edited) 3 hours ago, Morgan said: Super hard for me to see the pics are small to my eyes but looks like it could just me as simple as brushing on a white matte glaze unevenly/thin/thick and maybe a brushed cobalt wash? Could be underglaze but seems more like a wash from afar. +1 After a little googling, this looks similar: https://www.thepostsupply.com/products/vase-no-8 I got largest image I could access from that page by opening this image into another window -- then clicking on it to enlarge it further. https://www.thepostsupply.com/cdn/shop/files/AnemoneVaseno.8_Red_1024x1024@2x.jpg Similar treatment for this one. https://www.thepostsupply.com/cdn/shop/files/AnemoneVaseno.8_main_1024x1024@2x.jpg Edited November 27, 2023 by PeterH Min 1 Quote Link to comment Share on other sites More sharing options...
Min Posted November 27, 2023 Report Share Posted November 27, 2023 Looks like the base glaze was applied with a hake brush. Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.