Chiv Posted August 5, 2023 Report Share Posted August 5, 2023 Hi all, I couldn't find any threads on sealing finished work - do direct me there if there is ! I've been making work with parian and love it, I'm trying to go larger and experimenting with different uses. However I wanted to query if there was a seal that I could be using to help protect the surface. I'm not interested in glazing, as I like the surface as is. My work is predominately decorative but should I experiment with some functional pieces I'm also keen to know about sealing that's food safe. I don't want to add too much of a shine to the surface/alter its look too dramatically - as close to the raw/natural look of the fired clay surface as possible.. Any ideas? Also most of my experience has been with handbuilding black stoneware, again I love to keep them raw, matt, without a glaze on the surface - however, again I wonder if there is a seal I should/could be using to help prevent dust build up etc. and protect it without taking away from the surface and not adding shine. Thanks in advance!! D Quote Link to comment Share on other sites More sharing options...
Hulk Posted August 5, 2023 Report Share Posted August 5, 2023 Tough question! Parian* is generally defined as a "self-glazing porcelain" which appears to have nearly zero absorption. How are you using Parian? Do your finished wares absorb water, at all? *Composing a Workable Parian Clay Body (ceramicartsnetwork.org) Rae Reich, Chiv and PeterH 3 Quote Link to comment Share on other sites More sharing options...
Rae Reich Posted August 6, 2023 Report Share Posted August 6, 2023 (edited) I have some old china dolls and a few newer black clay pieces. I’ve always cleaned them with mild soap and water. I imagine that large, pale Parian surfaces which are not cleaned often might acquire some stains that could be hard to remove, but the relative non-absorbency should prevent most permanent staining. There are removers for rust stains that should work on Parian (test first on inconspicuous spot) and other types of dedicated cleaners for other stains. Vinegar and water would be my first attempt. Hydrogen Peroxide solution also, for mild bleaching without damage. The beautiful Wedgewood dinnerware is made of Parian, with no additional glaze. I wouldn’t leave my blueberry cobbler sitting on it overnight, though. Edited August 6, 2023 by Rae Reich Hulk and Babs 2 Quote Link to comment Share on other sites More sharing options...
Chiv Posted November 10, 2023 Author Report Share Posted November 10, 2023 @Hulk & @Rae Reich - thank you for your responses! I'm having trouble with this forum not letting me know I've had any replies, so I'm sorry not to have seen this! Glad to have some confidence about the parian surface. The pieces are mainly decorative, but I was also interested in experimenting with plants in some. I've not had trouble with water absorbing in general but wanted to know if there was anything else I should be thinking about to protect the 'white' surface for as long as possible. Re. my unglazed stoneware question, I'll try and ask where it's more relevant as still would like to know what best to do for protecting those pieces. Rae Reich and Hulk 2 Quote Link to comment Share on other sites More sharing options...
Chiv Posted November 10, 2023 Author Report Share Posted November 10, 2023 (Just to say that I now am receiving alerts, so thanks for the thumbs up @Hulk hah, good to know it's working!) Hulk 1 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.