Underglaze and Single Fire?


JayJ

Recommended Posts

  • JayJ changed the title to Underglaze and Single Fire?

Better imo to apply underglaze when leatherhard, then glaze when bonedry , dry and fire through to glaze maturity.

Pots turn out just fine.

@oldlady single fires her pots perhaps she will chip in here.

Quite comon , really. I learned the orocess and came uo caling it Raw Glazing, there are other names around.

 

Link to comment