danielle Posted October 24, 2022 Report Share Posted October 24, 2022 I have an old kiln I have no idea of manufacturer but my elements do not run on top of each other in a straight line they run side by side so it goes in the kiln and comes back out in the kiln on the same row all the way down and I cannot figure out how to wire it up and I cannot find any information on it and the plug I have only has NL 1 2 3 on it how do I hook the elements up to the switch I can only find information on whether in a straight line up and down mine aren't like that Quote Link to comment Share on other sites More sharing options...
oldlady Posted October 24, 2022 Report Share Posted October 24, 2022 danielle, welcome to the forum. we have several kiln experts here but they will need a lot more info to help you. can you post photos of everything about your kiln to help identify it? if there is writing at all on the exterior case, take a photo. look in all the places the info may be, along the sides of the box on the front where the knobs are. is it an old square one or is it many sided? photos of the exterior and some of the interior, size of the interior, photos of the elements themselves. is it loaded from the top or from the side? where did you get it and are you a new owner? someone can help you if you give all this info. Pres and Hulk 2 Quote Link to comment Share on other sites More sharing options...
danielle Posted October 24, 2022 Author Report Share Posted October 24, 2022 My phone won't let me send pictures Quote Link to comment Share on other sites More sharing options...
LostClay Posted October 24, 2022 Report Share Posted October 24, 2022 You can not upload pictures to the site? Quote Link to comment Share on other sites More sharing options...
neilestrick Posted October 25, 2022 Report Share Posted October 25, 2022 We really need pictures to help figure this out. Try emailing the pics to yourself to resize them. Quote Link to comment Share on other sites More sharing options...