Jtsonday Posted March 22, 2021 Report Share Posted March 22, 2021 What am I doing wrong? Link to comment Share on other sites More sharing options...
liambesaw Posted March 22, 2021 Report Share Posted March 22, 2021 Looks like some drying issues. Try to dry slowly, remove from the bat at leather hard, dry on the rim if possible. Link to comment Share on other sites More sharing options...
Jtsonday Posted March 22, 2021 Author Report Share Posted March 22, 2021 Thank you. I’ll try that. Link to comment Share on other sites More sharing options...
Mark C. Posted March 22, 2021 Report Share Posted March 22, 2021 Also try less water while throwing and get all the water off bottoms when form is done on wheel. Compressing bottom more will help as well. Link to comment Share on other sites More sharing options...
GEP Posted March 22, 2021 Report Share Posted March 22, 2021 Break those pots fully in half, and I bet you’ll find a big difference in thickness between the walls and the floor. This is an addendum to the above “uneven drying” answer. Evenly thick pots will dry evenly. Link to comment Share on other sites More sharing options...
Min Posted March 22, 2021 Report Share Posted March 22, 2021 Took the liberty of editing the title of this thread to better reflect the content. Link to comment Share on other sites More sharing options...
Rebekah Krieger Posted March 25, 2021 Report Share Posted March 25, 2021 Uneven drying for sure. Cover your pots loosely until it’s safe to flip over: then flip and cover a little tighter for a couple days before you remove plastic. Difference in thickness causes uneven drying. Link to comment Share on other sites More sharing options...