Amelia Posted October 10, 2020 Report Share Posted October 10, 2020 Anyone have thoughts or tips on refiring a bowl with a small spot that has crawled ? I’m pretty sure I just glazed it a little thick in that area (I haven’t had any crawling with this glaze- hundreds of pots later). Thinking I can just apply some glaze to patch the spot and refire? But not sure if once it crawls, there is no fixing. Any tips appreciated! Thanks!! Link to comment Share on other sites More sharing options...
liambesaw Posted October 10, 2020 Report Share Posted October 10, 2020 Looks like a stiff glaze so you will probably be able to see the spot you patch after, but there's no harm in trying. Link to comment Share on other sites More sharing options...
Amelia Posted October 10, 2020 Author Report Share Posted October 10, 2020 Thanks @liambesaw! Link to comment Share on other sites More sharing options...
Babs Posted October 10, 2020 Report Share Posted October 10, 2020 1 hour ago, Amelia said: Thanks @liambesaw! Helps to heat the pot and slightly thicker glaze Link to comment Share on other sites More sharing options...
Amelia Posted October 10, 2020 Author Report Share Posted October 10, 2020 @Babsthanks for the tip! Link to comment Share on other sites More sharing options...
Chilly Posted October 12, 2020 Report Share Posted October 12, 2020 Please let us know what happens.......... Link to comment Share on other sites More sharing options...
Denice Posted October 12, 2020 Report Share Posted October 12, 2020 I find that grinding the area with a stone on a Dremel tool, just roughing up the surface makes a big difference. I just did that to some small tiles that had a stiff glaze. Denice Link to comment Share on other sites More sharing options...