belamonk Posted February 3, 2020 Report Share Posted February 3, 2020 Recs for whitest stoneware clay from Laguna (northeastern). Thank you. Link to comment Share on other sites More sharing options...
Min Posted February 11, 2020 Report Share Posted February 11, 2020 Laguna sells sampler boxes of clay, you could check with your supplier and see if they would bring one if for you. It looks like there are only 3 light coloured cone 6 clays in the sampler box though, more for cone 10. What cone clay are you looking for? Hopefully someone who uses Laguna (northeastern) will chime in here for some suggestions. Welcome to the forum. Link to comment Share on other sites More sharing options...
oldlady Posted February 12, 2020 Report Share Posted February 12, 2020 may i ask why you are limiting your choices to just laguna? there are so many places to buy clay in the northeast of the USA if that is where you are. Link to comment Share on other sites More sharing options...
CactusPots Posted February 16, 2020 Report Share Posted February 16, 2020 The whitest Laguna stoneware on the west coast anyway is WSO. Link to comment Share on other sites More sharing options...
markalolo Posted February 20, 2020 Report Share Posted February 20, 2020 Miller #65 is pretty white. I like it. https://www.axner.com/wc609.aspx Link to comment Share on other sites More sharing options...
Mark C. Posted February 21, 2020 Report Share Posted February 21, 2020 Most shops have a laguna sample board of fire tiles .Laguna supplies this board to their retail distributors WSO is not like any clay body you have used -Its porous as heck at least at cone 10 .What cone are you wanting to fire to? cone 6 or cone 10? If its cone 6 you will be limited on choices Link to comment Share on other sites More sharing options...