See all updates by Dave Earley
-
-
I have put together 2 waste oil suction nozzles with electrodes to fire this kiln but after several attempts it keeps stalling at around 1100 degrees F. I don't think it is an insulation problem as I built it the same way as at first which fired to cone 10 with a different burner setup. My best guess is the burners are not efficient enough to make the power needed. I shut it off at 3:00 AM and will look at it for other problems, ie some collapse inside etc.
I will probably invest in some gas burners and go with propane.
-