Waiting for big bowls to dry so I can trim after work
-
I'm in the same place with my Christmas order. Looking to trim them this afternoon. Rain tomorrow will slow the drying process...should be able to bisque this weekend. How did your 40 cup project wind up?
-
All things considered the mugs went well, I think I lost 12, 2 handles popped, a few had tiny cracks and a few hadĀ glaze issues. Made more since then and I have a dozen more already bisqued and ready to glaze.
I have problems with my large bowls getting a tiny little crack in the bottom or warped rims, hoping this set of 6 will not have any issues
-