I forget how nice throwing porcelain is. Bought a bag of 365, never have tried it before. very nice indeed.
- Show previous comments 3 more
-
Standard
-
Did you all already tried to throw with Southern Ice? Absolutely best porcelain to throw, ever!
-
I haven't. The main reason for buying a bag was to try a glaze combination out that I really enjoyed on stoneware, hoping it would be brighter on porcelain. It ended up being a lot more boring on porcelain as the iron from the stoneware body comes out into the glazes and makes the much more interesting. So I will probably just turn the rest of the bag into slip.