  1. Picked up my compressor and sprayers today. Going to hook it all up tomorrow and start practicing. Really excited about the ability to control my glaze application a lot more than dipping and brushing.

    1. Show previous comments  9 more
    2. Joseph Fireborn

      Joseph Fireborn

      Welp. Sprayed for the first time after breaking in my compressor etc. It is interesting. Going to take some practice to get used to the movements and spray gun techniques. I like the low amount of glaze I have to have on hand though. I made some tall cylinders to practice on then fire to see how each different application comes out.

    3. glazenerd

      glazenerd

      High Volume Low Pressure. Remember, low pressure coming into the gun.

    4. Joseph Fireborn

      Joseph Fireborn

      Yea I kept the pressure at around 25 coming into the gun.

×
×