Firing over 200 test tiles in the next few days over 4 glaze firings. Normal Slow Glaze ^6, Slow Glaze ^5+1Hour Hold, Slow Glaze ^6 + slow cool, Slow Glaze ^6 super slow cool. Want to see all the variants of the same glazes and how they behave differently. Should be interesting.
- Show previous comments 12 more
-
Some good looking glazes in the gallery Have you called them variation glazes or are they variegation glaze? Not easy with a bit of dyslexia.
-
I dunno. Variation glazes because they add variety to my pots? I dont even know what variegation means lol... sorry for the confusion I will just change them to glazes.
-
Variegation is where the glaze splits into two different glass probably because of titanium.