Glaze firing test schedule #6 for surface qualities. Almost there.
-
I DID IT! After about 20 test firings with tweaking of glazes, bisque firing, and glaze firing. I finally have glossy glazes that I am proud to say are mine. Not only that but I achieved some beautiful results. I also solved my black clay bloating issue at the same time. Only took 5 months of work.
-