  1. Found a new glaze I like, that matches my base glaze. A deep red with speckles of black where it breaks. Also switching to frost porcelain so lots of new changes. Testing TIME!

    1. Show previous comments  3 more
    2. Joseph Fireborn

      Joseph Fireborn

      I mixed it. It is darker in room light, but in the sunlight that is how it looks.

    3. Joseph Fireborn

      Joseph Fireborn

      I will PM you recipe.