Firing over 200 test tiles in the next few days over 4 glaze firings. Normal Slow Glaze ^6, Slow Glaze ^5+1Hour Hold, Slow Glaze ^6 + slow cool, Slow Glaze ^6 super slow cool. Want to see all the variants of the same glazes and how they behave differently. Should be interesting.
- Show previous comments 3 more
-
I have never been able to convince myself to make duplicate tiles xD
-
You mean throw them, or just glazing the same tile with a glaze on a different schedule?
-
Yea putting the same glaze through different firing schedules