Been on a pottery hiatus due to some frustrations. Diving back in today!
- Show previous comments 1 more
-
Cannon Ball.
I had a million pots already made and bisqued. I glazed them and my kiln is in the slow cool process right now. I decided to try a new schedule with a long slow cool from 1750 to 1400. Looking for more of a satin finish as I am not a big fan of the gloss. Hopefully it will come out nice.
-
Sometimes taking a break gives you time to think things through, clear your head. Hope all goes well for you!
-
It came out well. I think I have some stuff to work with for a while. Posted the results on my gallery of my 3 favorite pieces.