Firing over 200 test tiles in the next few days over 4 glaze firings. Normal Slow Glaze ^6, Slow Glaze ^5+1Hour Hold, Slow Glaze ^6 + slow cool, Slow Glaze ^6 super slow cool. Want to see all the variants of the same glazes and how they behave differently. Should be interesting.
- Show previous comments 6 more
-
Yea, I haven't done it before either, but I feel like having the 4 tiles from different schedules will help me understand a lot more. I will definitely post the results on my gallery once I have all 4 of the tiles side by side. I assume there will be a lot of difference in some.
-
First set of glaze tiles out of the kiln. I will post pictures shortly to my gallery got a few things to handle and I am going to ge the second load in the kiln and started.
-
Must be an amazing experience!!