  1. Glazing 40+ test tile cones with different applications, brush marks, finger marks, watered down layered glazes, and RIO. Sometimes 4-5 layers! Should be interesting, or terrible.

    1. Show previous comments  7 more
    2. GiselleNo5

      GiselleNo5

      Also, faux ash glazes might achieve some of that special effect like you want.

    3. Joseph Fireborn

      Joseph Fireborn

      I use red rock it MnO specs that come through in the glazes.

    4. Marko

      Marko

      I've been sick these past few days. So how did the test come out?