  1. just made some plaster molds while waiting to trim some porcelain pieces.

  2. Marcia Selsor

    sculpture

  3. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    more ferric chloride, manganese and copper with some sugar granules and silver nitrate granules.
  4. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    another one with manganese salts
  5. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    This was too large for my saggars so I foil saggar fired it.
  6. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    this one had some manganese salts sprayed over copper and ferric chloride
  7. Just fired saggar. Pots for the third day. learning curve is growing. playing with sulphates and a cobalt alloy. just ordered a manganese salt.

  8. Welcome to the forum. This should kit start your experiences with clay. Life is short so make the most of it. Take some workshops. You can get a lot out of them.

    Marcia

  9. It is in the comment of the green plate preceding this jpg. M
  10. so you are in the UK. Thanks for letting me know.

    Marcia

  11. Thanks for the posting photo review. I brightened mine up.

    Marcia

×
×