  1. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    experimenting with textured surfaces for Obvara firings
  2. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    experimenting with textured surfaces for Obvara firings
  3. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    experimenting with textured surfaces for Obvara firings
  4. that should say flour solution or liquid Marcia
  5. Pressure is on to get everything shipped asap.

    1. trina

      trina

      sounds like you should drink a lovely cup of tea!

    2. Evelyne Schoenmann
  6. Jury duty is over. Back to the studio.

  7. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Hot pot coming out of Flour paste brew.
  8. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.
  9. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water. Pieces cooling
  10. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.
  11. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.
  12. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.
  13. From the album: saggar, horse hair, feathers, foil saggars, Obvara

    Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.
  14. Fired Obvara today successfully. will post pics in the gallery!

    1. Evelyne Schoenmann

      Evelyne Schoenmann

      Beautiful pieces Marcia!

    2. trina

      trina

      wow those are great!

       

  15. Porcelain tends to fuse to itself during the glaze firing. Sometimes the feet also fuse to the kiln shelf. So using Alumina prevents both of these things from happening. Marcia
  16. I use less too. But I add it to diluted wax. Probably about 2 tsp to 8 oz. Marcia
  17. That's possible. I dilute the blue wax to get it to brush on easily. Did you dilute your wax? Marcia
  18. I have used alumina in wax on porcelain for many years and never saw anything like that. I usually just brush is one both sides and the bottom for porcelain. I can only think that it may have dripped during application. Was your wax white? For that process, I use the Aftosa wax. I like it because it is bluish and can be seen. It can come off if you make a mistake and catch it immediately. Marcia
  19. waiting for the wind to die down so I can fire.

×
×