finished two raku kilns yesterday but not the flashing idea. These are oil drum kilns with 1/3 cut off. Also added a burner holder. One is a replacement for my smaller raku kiln and the other is for a friend. the flashing ended up around the grapefruit trees for protection against rates. It seems to be working.
-
such sacrifices :-))) industrious person!
-
I posted pictures in my gallery under kilns