I mixed clay today! Picked up dry clays about 11, did errands, and started mixing about 1 pm while the sun was warm . Cold front is coming in tonight. Beat it! So happy. Mixed about 270 pounds wet. That should be a good start. This batch is for making new saggers. I didn't bring many with me. My birthday is Wed. so I can celebrate by doing some throwing. Kilns will be getting wired in Mid- February.
- Show previous comments 5 more
-
they are for my low temp. I will bisque to 08 and fire with pots to the same.
-
Happy Birthday!!
-
Nothing better than working in your new cozy studio while the winter blasts away outside your door. Happy Birthday.