Denice
-
Posts
2,397 -
Joined
-
Last visited
Reputation Activity
-
-
-
Denice reacted to LeeU for a gallery image, HMS No. 5 Emerging
This piece was fired in the anagama kiln at the Sharon Art Center in NH. It is porcelain with a celedon glaze on the facial planes and a temmoku on the stamped area. The orange on the right side is on unglazed clay and is an attribute of the firing.
-
Denice reacted to 1515art for a gallery image, Desert night to day
Hunting for gold among the rock and sage
-
Denice reacted to Celia UK for a gallery image, White earthenware 'shell' bowl
Thrown white earthenware, linear additions, Holes carved then dots added. Wash of copper oxide and cobalt carbonate airbrushed when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.
-
-
Denice got a reaction from Miss B for a gallery image, 3 Spill fountain
9.5ft tall 5ft wide tallavera tile, cone 1 majolica, spills and molding cone 6 stoneware
-
-
-
-
Denice reacted to rakukuku for a gallery image, heart pink Pic
here is a product of yesterday's naked raku one step. pink terra sig. i added more alumina hydrate to the slip and we got the right amount of adherence. rakuku
-
Denice got a reaction from jolieo for a gallery image, 3 Spill fountain
9.5ft tall 5ft wide tallavera tile, cone 1 majolica, spills and molding cone 6 stoneware
-
-
-
Denice reacted to Marcia Selsor for a gallery image, cone 6 Faux Celedon
Selsor Faux Celedon ^6 Oxidation
Whiting 18.5
Neph Syen 25.8
EPK 18.8
Silica 31.1
Gerstley B 4.6
98.8
Copper carb 0.3
Mason #6600 Black 0.02
-