A wood duck mug made as a gift for a lady's husband for Xmas.

I cannot believe how wonderfully bright these colors turned out! The terracotta didn't alter the underglaze at all. Soooo happy with this chubby lil' guy!

 

Seward terracotta, Clay Art Center underglaze, Mayco underglaze, Mason Stain

Fired to ^03.

Copyright

© Cavy Fire Studios
From the album:

Late 2015

  • 6 images
  • 0 comments
  • 25 image comments

Photo Information for Wood Duck Mug

 Share


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.