Posted 03 April 2013 - 10:07 AM

I was mentioning to Niel that I got a box of A.R.T's Ultra Brownstone - It looks even darker than the pictures indicate after being fired. Literally like chocolate. Anyways I have fallen in love with the feel of this clay body. I saw a sample at the shop that had pink chiffon glaze over that dark and it looked like a burny dark green brown. It's intimidating to think of glaze and how it will react over such a strong clay body. Can anyone point me in the direction of potters who use a super dark clay so I can catch some inspiration?

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#2 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 03 April 2013 - 10:25 AM

I was mentioning to Niel that I got a box of A.R.T's Ultra Brownstone - It looks even darker than the pictures indicate after being fired. Literally like chocolate. Anyways I have fallen in love with the feel of this clay body. I saw a sample at the shop that had pink chiffon glaze over that dark and it looked like a burny dark green brown. It's intimidating to think of glaze and how it will react over such a strong clay body. Can anyone point me in the direction of potters who use a super dark clay so I can catch some inspiration?


ack- I called them and It sounds like only a handful of people use this clay body because it is New - it just came out less than a year ago.

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,111 posts
  • LocationRaleigh, NC

Posted 03 April 2013 - 10:43 AM

If you like the feel of this clay, chances are others will too so you might want to leave clay exposed on outer surfaces or find glazes that break and let the clay show through. There are some nice 'oatmeal' glazes that work well with dark clays but often these clays look best when allowed to take center stage. Just an opinion however!
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,325 posts
  • LocationRed Lodge, Montana

Posted 03 April 2013 - 12:45 PM

I like dark bodies for sgraffito. I use a porcelain slip made from my trimmings. when I was in France. There was a black body over there.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 03 April 2013 - 04:17 PM

I loves me some dark clay. (Studio owner not so much)

I use standard 266 a lot. It is dark but not black. Looks somewhat similar from what I can tell from on line image.

I don t see a lot of people using dark clay, I am also interested in seeing others work in dark clay.

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#6 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 03 April 2013 - 10:59 PM

would any of you be able to share some pictures of your dark clay pieces for inspiration? :)

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#7 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 04 April 2013 - 01:38 AM

No pictures yet, but I've got a piece in the kiln now out of Laguna's Electric Brown (nice n chocolatey!) where I textured the surface with a stone and then hit it with red iron oxide after bisquing... I've done it in the past and it comes out a lot of fun!
Maryjane Carlson

Whistling Fish Pottery

#8 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 04 April 2013 - 12:52 PM

would any of you be able to share some pictures of your dark clay pieces for inspiration? :)/>/>/>/>/>


Here you go

5 inch, eastern inspired small plate,dish, hand formed, standard 266 clay with added grog, black and white slip transfer, zen influenced enso design, under a clear glaze, fired cone 6 ox.
The dark clay excels when it has a voice in the design.

Second image

11 x 4.5 inch stretched plate. With a transparent green glaze, oribe inspired, The dark clay acts as earthy palette for the glaze, and there is interesting color transitions from dark green , to transparent green, earthy browns and reds, to pools of black.

Attached Files


LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#9 Natania

Natania

    Advanced Member

  • Members
  • PipPipPip
  • 200 posts
  • LocationMassachusetts

Posted 04 April 2013 - 01:23 PM

Here are some pieces I made with standard 266. I use a glaze called "Cream breaking red" and fire to cone 5. I will post the glaze recipe when I find it (I left my glaze notebook at school where I teach)....I apply the glaze quite thinly to get more of the clay color showing through...I would love to find a creamy white that shows up on this clay, but I can't imagine there is one that would work...

Attached Files


  • mss likes this

#10 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,264 posts
  • LocationWilton, NH USA

Posted 04 April 2013 - 03:41 PM

Among a number of others, I use a very dark body (Sheffield Pottery #42 which contains a lot of Lizella and the local Sheffield earthenware slip clay) to which I add in NH granite dust/chunks. It is reated cone 8 oxidation... I fire to to cone 10-14 woodfire reduction.......but only for smaller forms... large ones don't like all the heat and reduction. Often with a nuka (rice husk ash) glaze and then sometimes overglaze enamels.

Tea Caddy and Yunomi

best,



...............john



PS... running out of image upload quota.

Attached File  Baymore-TeaCaddy-1024x768.jpg   512.85KB   189 downloads

Attached File  Baymore-Yunomi-IMG_8669-1024x768.jpg   707.9KB   153 downloads

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#11 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 04 April 2013 - 04:59 PM

Among a number of others, I use a very dark body (Sheffield Pottery #42 which contains a lot of Lizella and the local Sheffield earthenware slip clay) to which I add in NH granite dust/chunks. It is reated cone 8 oxidation... I fire to to cone 10-14 woodfire reduction.......but only for smaller forms... large ones don't like all the heat and reduction. Often with a nuka (rice husk ash) glaze and then sometimes overglaze enamels.

Tea Caddy and Yunomi

best,


...............john


PS... running out of image upload quota.

Attached File  Baymore-TeaCaddy-1024x768.jpg   512.85KB   189 downloads

Attached File  Baymore-Yunomi-IMG_8669-1024x768.jpg   707.9KB   153 downloads


Nice! I especially like the yunomi. And to think a little of my home town is in those pots. Lizella is dug way back in the swamp on Echoconnee Creek where I grew up swimming with water moccassins and sleeping on sandbars in the middle of the creek eating robins and eels. What is the lid to the tea caddy?

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#12 deborah.

deborah.

    Newbie

  • Members
  • Pip
  • 7 posts
  • LocationBlacksburg, VA

Posted 04 April 2013 - 09:39 PM

I'm a pretty new, young potter (one extensive year in). First time poster but have been reading the forums for the past few months. This bowl is glazed with one of the studio's house glazes overlapping in the middle the Fall's Creek Shino glaze (Recipe) on Standard's 266 clay body.

Attached Files



#13 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,264 posts
  • LocationWilton, NH USA

Posted 04 April 2013 - 10:56 PM

What is the lid to the tea caddy?


Thanks for the positive feedback, Jim.

The lids for my darker clay chaire are usually unglazed porcelain. On the porcelain chaire, they are the dark Lizella based body. Occasionally I use (fossil) ivory.

best,

..................john

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#14 Pompots

Pompots

    Advanced Member

  • Members
  • PipPipPip
  • 104 posts
  • LocationCalifornia

Posted 05 April 2013 - 02:55 AM

I use mostly cone 5 Nara Porcelain, but sometimes I use Cassius Basaltic from Aardvark Clay in Santa Ana, CA. It is a very nice and smooth clay wonderful for throwing. The glaze is Pink Ice from Laguna Clay Co, City of Industry, CA

Attached Files



#15 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 05 April 2013 - 07:51 AM

Among a number of others, I use a very dark body (Sheffield Pottery #42 which contains a lot of Lizella and the local Sheffield earthenware slip clay) to which I add in NH granite dust/chunks. It is reated cone 8 oxidation... I fire to to cone 10-14 woodfire reduction.......but only for smaller forms... large ones don't like all the heat and reduction. Often with a nuka (rice husk ash) glaze and then sometimes overglaze enamels.

Tea Caddy and Yunomi

best,



...............john



PS... running out of image upload quota.

Attached File  Baymore-TeaCaddy-1024x768.jpg   512.85KB   189 downloads

Attached File  Baymore-Yunomi-IMG_8669-1024x768.jpg   707.9KB   153 downloads


Is the glaze on the top half of the Tea Caddy ash from the firing or an applied glaze?

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#16 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,264 posts
  • LocationWilton, NH USA

Posted 05 April 2013 - 09:48 AM

Is the glaze on the top half of the Tea Caddy ash from the firing or an applied glaze?


Jim,

A combination of fine flyash (fired in a location in the noborigama well away from the firebox) as well as my applied Oribe glaze. The clay body below that is all "fumed" from the volatiles coming from the wood ash in the general chamber environment (no salt or soda added).

best,

..............john

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#17 Clay 4 All

Clay 4 All

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 09 April 2013 - 05:47 PM

You might want to check out Stone Mountain Clay out of Georgia. They have a black clay "onyx Krunch" Stoneware cone 6.
Just saw a glazed piece today and it was black.

I have used 266 with nice results but not as dark as the onyx crunch...

I agree with one of the earlier posts, slips might be the ticket when working with
these clay bodies of this color.

#18 bigDave

bigDave

    Advanced Member

  • Members
  • PipPipPip
  • 89 posts
  • LocationSo-Cal

Posted 12 April 2013 - 10:25 PM

would any of you be able to share some pictures of your dark clay pieces for inspiration? Posted Image


Cant imagine its much of an inspiration, but 80% or so of what I make is of electric brown, non glazed


Bonsai,

big d

Attached Files



#19 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 15 April 2013 - 10:19 AM


would any of you be able to share some pictures of your dark clay pieces for inspiration? Posted Image


Cant imagine its much of an inspiration, but 80% or so of what I make is of electric brown, non glazed


Bonsai,

big d


And thank you for providing me with my pottery porn for the day!! DROOLING over your collection!

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#20 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 15 April 2013 - 10:21 AM

Among a number of others, I use a very dark body (Sheffield Pottery #42 which contains a lot of Lizella and the local Sheffield earthenware slip clay) to which I add in NH granite dust/chunks. It is reated cone 8 oxidation... I fire to to cone 10-14 woodfire reduction.......but only for smaller forms... large ones don't like all the heat and reduction. Often with a nuka (rice husk ash) glaze and then sometimes overglaze enamels.

Tea Caddy and Yunomi

best,



...............john



PS... running out of image upload quota.

Attached File  Baymore-TeaCaddy-1024x768.jpg   512.85KB   189 downloads

Attached File  Baymore-Yunomi-IMG_8669-1024x768.jpg   707.9KB   153 downloads


Gorgeous!!

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users