yedrow Posted January 15, 2013 Report Share Posted January 15, 2013 Okay, it isn't earth shattering, but it seems to be a decent glaze. I think I need to flux it a little more to get what I want. Link to comment Share on other sites More sharing options...
Brian Reed Posted January 15, 2013 Report Share Posted January 15, 2013 Nice I like the transparent breaking on the rim. Link to comment Share on other sites More sharing options...
SmartsyArtsy Posted January 15, 2013 Report Share Posted January 15, 2013 Very nice, yedrow. I like the depth. Do you have rutile or ilmenite in it? Link to comment Share on other sites More sharing options...
Hermes Posted January 15, 2013 Report Share Posted January 15, 2013 Okay, it isn't earth shattering, but it seems to be a decent glaze. I think I need to flux it a little more to get what I want. I think this is a more than decent glaze. Hermes Link to comment Share on other sites More sharing options...
atanzey Posted January 15, 2013 Report Share Posted January 15, 2013 I LIKE it! You may inspire me to try my own formulations! (With the help of a program, of course). Are you going to be interested in sharing? ;-) Alice Link to comment Share on other sites More sharing options...
Marcia Selsor Posted January 15, 2013 Report Share Posted January 15, 2013 I like the surface. The color is not for me , but it is a nice surface and breaking color change. Very decent indeed!!! Marcia Link to comment Share on other sites More sharing options...
minspargal Posted January 15, 2013 Report Share Posted January 15, 2013 Oh very nice glaze, reminds me of the rutile blue glaze we used to use at school. Link to comment Share on other sites More sharing options...
TJR Posted January 15, 2013 Report Share Posted January 15, 2013 yedrow; What is it you are trying to achieve? If you fluxed it more, it will run more. I like the colour and surface. Keep going! TJR. Link to comment Share on other sites More sharing options...
yedrow Posted January 15, 2013 Author Report Share Posted January 15, 2013 Thank you Brian! Thank you Chris, it has rutile in it. Thank you Hermes, you helped!!! Thank you Alice, I'm going to share some, but as I put my pallet together I'll probably get a little stingy, at least for a couple of years. I'm not very good at being stingy though. Thank you Marcia! Thank you minspargal, good eye. TJR, it has some dry spots in the glaze that I think would come out if it were fluxed better or fired longer. However, I'm pushing the body at present so I'm thinking I need to go the more fluxing route. I'm really digging this glaze stuff. I've been working hard the last year to understand glazes and their chemistry. With Hermes help I got a much better understanding, and the Britt video really helped me in adjusting application. And being on this board with all the great talent and knowledge, and with those like me who are developing potters, has helped a great deal. Thanks all, Joel. Link to comment Share on other sites More sharing options...