Brain Picking Time,

And dont tell me that its slim pickins as I know full well there is a wealth of knowledge out there.Posted Image
I am thinking of doing a large number of pieces that need to have a repetive graphic. Something not to detailed but is stamped one image at a time.
So am wondering if anyone has any experience using diluted Mason stain as an ink for a stamp pad. I have looked at the forums and havent quite found exactly what I am looking for. I would be using a rubber stamp of my own design. If there is something better for this process or is there an ink that would withstand ^6 firing. I would sure appreciate learning about it. I will be working on Porcelain and Stoneware.

Thanks in advance,

RJ

#2 JLowes

JLowes

    Clay Doodler

  • Members
  • PipPipPip
  • 266 posts
  • LocationAtlanta Georgia area

Posted 14 September 2012 - 11:58 AM

Check out this link. There is discussion of how to make ceramic ink using Mason stain:

http://ceramicartsda...images-on-clay/

I would expect that putting your homemade ink on a pad and using a brayer to transfer the ink to your stamp would be the best. A few experiments would educate you on that.

I have some linseed oil and Mason stains at home, so maybe I should try this myself (thanks for the inspiration.)


John

#3 Wind n Wing

Wind n Wing

    Advanced Member

  • Members
  • PipPipPip
  • 62 posts

Posted 14 September 2012 - 12:30 PM

Check out this link. There is discussion of how to make ceramic ink using Mason stain:

http://ceramicartsda...images-on-clay/

I would expect that putting your homemade ink on a pad and using a brayer to transfer the ink to your stamp would be the best. A few experiments would educate you on that.

I have some linseed oil and Mason stains at home, so maybe I should try this myself (thanks for the inspiration.)


John


John,
The link you suggested is tickling my grey, very grey cells. But my curiosity is being peaked by your mention of Linseed oil and Mason stains. Can you give me more info on this.
Thanks,
RJ

#4 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,304 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 14 September 2012 - 01:53 PM

Just about any colorant works well with stamps on clay on ink pads-I have used many-Iron and cobalt for sure.
As to mason stains which I use some i see no reason why not.
Mark
Mark Cortright
www.liscomhillpottery.com

#5 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,112 posts
  • LocationRaleigh, NC

Posted 14 September 2012 - 02:03 PM

Maybe you could use underglazes and just saturate a sponge to use as an ink pad?
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#6 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,304 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 14 September 2012 - 03:06 PM

As Chris mentioned you do not need a ink pad-a thin sponge will work even a rag.
Mark Cortright
www.liscomhillpottery.com

#7 macdoodle

macdoodle

    Advanced Member

  • Members
  • PipPipPip
  • 84 posts
  • LocationOrange County, CA, USA

Posted 14 September 2012 - 07:40 PM

You tube to the rescue-
and to make the stamps-

#8 Lucille Oka

Lucille Oka

    Advanced Member

  • Members
  • PipPipPip
  • 756 posts
  • LocationCalifornia

Posted 14 September 2012 - 07:52 PM

You can also check the Minnesota Clay Company they have underglaze stamp pads, underglaze carbon papers, underglaze markers lots of fun stuff. Some of these products have firing temperature limits so be sure to read the information. http://www.mnclay.co...otters_pad.html
John 3:16
"For God so loved the world that He gave His only begotten Son, that whosoever believeth in Him should not perish but have everlasting life".

#9 Wind n Wing

Wind n Wing

    Advanced Member

  • Members
  • PipPipPip
  • 62 posts

Posted 14 September 2012 - 09:55 PM

You have all been a great help. Thank you, Thank you. I am excited to try all the suggestions, so many choices and such a short lifetime. Think if I lived to be 1000 and tried something new there would still be eaons of things to learn. Love the Minn. clay site. You tube can consume me there are so many neat things to see. I will experiment with these suggestions and let you know what worked best.

Again

Thanks,

RJ

#10 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,176 posts
  • LocationCentral, PA

Posted 17 September 2012 - 01:13 PM

You have all been a great help. Thank you, Thank you. I am excited to try all the suggestions, so many choices and such a short lifetime. Think if I lived to be 1000 and tried something new there would still be eaons of things to learn. Love the Minn. clay site. You tube can consume me there are so many neat things to see. I will experiment with these suggestions and let you know what worked best.

Again

Thanks,

RJ


I have used sponges and ink pads in the past to stamp a rubber stamp symbol that contains text and graphics on my chalices and patens for a customer. I have used commercial pads, and my own. My own used commercial stains, iron oxide or cobalt mixed with linseed oil. I tried these on sponges, but found that I got too much ink. Later I tried gluing a think piece of felt on to a board, and inking the felt, pressing the stamp into the felt firmly and evenly gives me the clean image over glaze. I then atomize the stamped area with more glaze before firing. Be certain to make a thin ink, not really thick.
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#11 macdoodle

macdoodle

    Advanced Member

  • Members
  • PipPipPip
  • 84 posts
  • LocationOrange County, CA, USA

Posted 05 January 2013 - 02:10 AM

Wind n Wing

Make sure to show us what you make!




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users