So I have a bucket of black slip that I made out of some clay and it is in a thick "pudding" state. I want to thin some of it for brushwork or dipping. Knowing that if I add more water to this I stand the chance of it settling out or being too thin. Is a deflocculant the answer to keeping it suspended and at the right viscosity / specific gravity for application. I want to keep some of it thick for spreading and texture though. Thoughts?

Link to comment
Share on other sites

I like to deflocculate slips because they bond better and dry faster. In the past I used slips that I would do sgraffito work through, so I liked to apply them to pots that were on the dry side of leather hard. Without deflocculating, the slip was more likely to flake off, since I was doing three thick coats.

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.