  1. I clean after throwing to keep the dust down.  If I sweep or rather drag the broom, I have a spray bottle in my hand to also keep the dust down I empty the trimming & clean up the floor after trimming, so I keep the studio as free from dust as I can.  The studio is a small room in the basement.  My sink & glaze area is in the furnace/laundry/hallway to the studio so any drips get wiped up immediately to keep my pup from licking them.  

    I keep the studio washed up better than the rest of the house.  I do clean the rest once in a while.

    Joy

  2. I cut out stencils from thick tablecloth vinyl & use iron oxide to stamp.  I use a tub with folded jersey cloth for a pad to keep the amounts of oxide  just right for a stamping  foam brush the pad allows the oxide to fill the stamping tool but not too much.  I stamp on top of a glazes  as control of the oxide is essential,  too little & the stamp fires faded too much & it is dark & messy.  I periodically add water with a small squirt bottle for moisture.

    joy

  3. My skut kiln is almost 40 yrs. old & I just had new elements replace top to bottom for the 1st time. Have had sections replaced before. I glaze fire in a day & wonder if it will be just as before or fire higher. Reset the sitter by eye, just touching. It works better that way for me usually. Maybe I'd better wash the bottoms of the runnier glazes back further.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.