Mark C. Posted May 1 Report Share Posted May 1 Got a notice about this thru a few sources. Laguna has 2-3 other choices with Mahavir Feldspar being the go to Hard to say if this is permanent or will change again-if You like custar and need custar buy oit now while you can find it.-Last call Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Mark C. Posted May 3 Author Report Share Posted May 3 Laguna will be carring these potassium feldspars .Mahavir and Vardham from India and G-200 depending on availability Quote Link to comment Share on other sites More sharing options...
Min Posted May 3 Report Share Posted May 3 (edited) I have the analysis for Vardhman, I'll add a pinned thread on potash feldspar changes. edit: Pin link added here. https://community.ceramicartsdaily.org/topic/41698-potash-feldspar-comparisons-of-custer-mahavir-g200eu-and-vardhman/ Edited May 3 by Min Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted May 6 Report Share Posted May 6 I spoke with my supplier last week, and they said that Plainsman has a 4 year supply IF no one hoards it. Mike at Ceramics Canada has said he won’t sell more than a 50 lb bag at a time unless you’ve been making your own clay body with it. So please don’t panic buy. Give everyone ample time to reformulate behind the scenes while still using their current stock. Morgan and Min 2 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.