Potpotpotter Posted November 20, 2023 Report Share Posted November 20, 2023 Hello everyone! I use luster on some of my mugs on the outside only but I believe I put some on inside by accident and it went unnoticed Is there a way to get this out? Thanks! Quote Link to comment Share on other sites More sharing options...
Min Posted November 20, 2023 Report Share Posted November 20, 2023 Yup. A gold and luster eraser. https://tuckers-pottery-supplies-inc.shoplightspeed.com/gold-luster-eraser.html Rae Reich and LeeU 2 Quote Link to comment Share on other sites More sharing options...
Potpotpotter Posted November 20, 2023 Author Report Share Posted November 20, 2023 Oh wow I never knew something like this existed! Thank you Quote Link to comment Share on other sites More sharing options...
Pyewackette Posted November 21, 2023 Report Share Posted November 21, 2023 ok. Now I want to know how this works. At first I thought it must be melting point related but gold melts at a relatively low 1948F, which is around cone 04. Enquiring minds want to know ... Quote Link to comment Share on other sites More sharing options...
PeterH Posted November 21, 2023 Report Share Posted November 21, 2023 (edited) On 11/21/2023 at 3:10 AM, Pyewackette said: ok. Now I want to know how this works. At first I thought it must be melting point related but gold melts at a relatively low 1948F, which is around cone 04. Enquiring minds want to know ... From https://community.ceramicartsdaily.org/topic/1557-gold-lustre-and-alkaline-glaze/?do=findComment&comment=10521 1. Lustre is a thin film of metal deposited on the surface of a fired glaze. It is NOT a glaze in itself. It relies on the glaze interaction with the lustre for adherence and this can be anywhere between 720.C-820.C depending on the hardness of the glaze. Earthenware glazes are usually refired between 720-750.C while stoneware and porcelain usually refire between 780-820.C but that is not set in stone. Every glaze is different and you would have to test to find the common denominator for your glazes. Glass, depending on the type, starts to accept lustre from 600.c onwards. You will know if you haven't fired high enough as the lustre will rub off. If fired too high it will start to burn off and be patchy. Commercial porcelain blanks can be tricky to find the optimum temperature as a lot of these follow the procedure of high fired bisque with a low fired glaze. This appears to be the same with bone china. It takes on the characteristics of the glaze it is on. If the the glaze is very glossy then the metallic layer is very glossy. If the glaze is matt then the metal layer is matt and this then follows on for all the permutations in between. However I have noticed in my own work that copper glazes seem to be more problematic as my lustres always seem duller. This then brings me to the second point. PS These lustres (there are reduction lustres as well) are based on resinates, which are metallic soaps. When they are heated they decompose to metal atoms and various gases such as CO2. Why most of them (e.g. copper) don't decompose to the oxide is complex, and apparently relates to the electron distribution within the resinate ion during its decomposition. Which is why resinates are still used. Danger of skin contact & fumes until they are fully fired, then you've got a metallic thin film (somewhat amalgamated with the surface of the underlying glaze). Some of the dangers are inherent to the resinate, others relate to the solvents used. Johanna DeMaine Lustre Ceramics Monthly Health & Safety and Overglaze Background Overglaze: Challenging the Myths Edited November 27, 2023 by PeterH Pyewackette, Callie Beller Diesel and Min 3 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.