Biglou13 Posted November 3, 2023 Report Share Posted November 3, 2023 I’m finally able to get access to cone 10 firing Anyone have a recipe? Cone 10 redux, extra points if leans to traditional Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted November 4, 2023 Report Share Posted November 4, 2023 Hey Lou! Good to see you again! Not sure how traditional it is from a chemistry standpoint, but this glaze does tick a number of boxes around how Oribe’s are supposed to behave. It IS fluid, and tends to go metallic if on the interior of a bowl. Wouldn’t suggest it for food surfaces, but is a lovely accent bit. The bone ash does gel the glaze somewhat, so that will affect its application. I haven’t ever tried it in an acid bath after the firing, as I’ve seen some Japanese artists do since. Due to the age of this recipe, you may have to do some calculations to allow for material analysis shift, especially if you are buying talc new for this. Custer was also a different animal than it is now. Carolina Oribe (ACAD shop, circa 1998 or so) 29 Custer Feldspar 24 Silica 21 Whiting 12 EPK 7.5 Talc 1 Bone Ash 5.2 Copper Carb Quote Link to comment Share on other sites More sharing options...
neilestrick Posted November 4, 2023 Report Share Posted November 4, 2023 Oribe.pdf Quote Link to comment Share on other sites More sharing options...
Biglou13 Posted November 5, 2023 Author Report Share Posted November 5, 2023 On 11/3/2023 at 9:11 PM, Callie Beller Diesel said: Hey Lou! Good to see you again! Not sure how traditional it is from a chemistry standpoint, but this glaze does tick a number of boxes around how Oribe’s are supposed to behave. It IS fluid, and tends to go metallic if on the interior of a bowl. Wouldn’t suggest it for food surfaces, but is a lovely accent bit. The bone ash does gel the glaze somewhat, so that will affect its application. I haven’t ever tried it in an acid bath after the firing, as I’ve seen some Japanese artists do since. Due to the age of this recipe, you may have to do some calculations to allow for material analysis shift, especially if you are buying talc new for this. Custer was also a different animal than it is now. Carolina Oribe (ACAD shop, circa 1998 or so) 29 Custer Feldspar 24 Silica 21 Whiting 12 EPK 7.5 Talc 1 Bone Ash 5.2 Copper Carb Good to be back thanks. I have stash of some old school talc. Quote Link to comment Share on other sites More sharing options...
Biglou13 Posted November 5, 2023 Author Report Share Posted November 5, 2023 18 hours ago, neilestrick said: Oribe.pdf 56.3 kB · 3 downloads Thanks Neil ! Hulk and neilestrick 2 Quote Link to comment Share on other sites More sharing options...
Russ Posted November 5, 2023 Report Share Posted November 5, 2023 Hey @ biglou13 if you have old school talc then i would suggest a tea dust. Beautiful glaze and colorants can be added to acheive that dark green. Try John Britt's recipe. Quote Link to comment Share on other sites More sharing options...