Glaze chemicals got wet. Help?


Nors

Recommended Posts

Embarrassed that I have to ask this, but I had a box with various bags of newly purchased materials in my car and one of the back windows was left open and it rained overnight. (The child lock was deactivated. Argh.) 

Most are in plastic and therefore fine, but epk, minspar 200, and frit 3134 are in paper bags that got damp. 5 lb bags.  Should I be concerned? Are they fine to use? Should I decant into plastic bins and let dry a bit before closing up? How best to proceed? Thanks. 

Link to comment
Share on other sites

wish i had had this advice back in 1990 when i was building a house and studio.   3 or 4 fifty pound bags were wet and i left them on the ground where thay had fallen after delivery.  2 were frits 3124 and 34.  when the bags were finally dry enough to lift they were no longer rigid but i did not look closely enough before they were tossed in a trash truck and driven off.   what a loss that was.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.