neilestrick Posted February 11, 2023 Report Share Posted February 11, 2023 A wiring diagram sure would be nice! Can the manufacturer get one to you? High Bridge Pottery 1 Quote Link to comment Share on other sites More sharing options...
MartinC Posted February 13, 2023 Author Report Share Posted February 13, 2023 Have called Kilns & Furnaces to try and get a diagram neilestrick 1 Quote Link to comment Share on other sites More sharing options...
MartinC Posted February 14, 2023 Author Report Share Posted February 14, 2023 Looks like a safety override. Kiln errored with one hour of starting. Have disconnected it and am trying again Bill Kielb 1 Quote Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted February 14, 2023 Report Share Posted February 14, 2023 I wonder why it is overriding the firing. hmm The controller seems to be switching on and off the brown wire going to the weird black box and then that is switching the contactor. I wonder if you could just attach that brown wire to the coil instead of the yellow coming from the box as they both seem to be 240v. Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted February 14, 2023 Report Share Posted February 14, 2023 (edited) 1 hour ago, High Bridge Pottery said: e yellow coming from the box as they both seem to be 240v. Just jump the red to yellow at that switch to remove its function from the circuit. Supervise the firing for sure though. If it is wired as fail safe then the kiln will fire. If it triggers a lockout, then it will be locked out to start. Edited February 14, 2023 by Bill Kielb Quote Link to comment Share on other sites More sharing options...
MartinC Posted February 15, 2023 Author Report Share Posted February 15, 2023 So, with safety override in place, kiln errored at about 200oC. With it unplugged, kiln has now fired twice without error so Im think that's where the problem lay. It is superficial as the safety override now comes from the controller so I think the mystery is solved. Thank you to everyone for your engagement and help. High Bridge Pottery, neilestrick and Bill Kielb 3 Quote Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted February 15, 2023 Report Share Posted February 15, 2023 Glad you figured it out and happily firing again Always nice to solve a mystery. Quote Link to comment Share on other sites More sharing options...