Stumonster Clayworks Posted November 26, 2022 Report Share Posted November 26, 2022 Has anyone used tin oxide from us pigment? Compared to my local supplier, it is a quarter of the cost... is this because purity is not up to par? Thanks, Stuart Quote Link to comment Share on other sites More sharing options...
Mark C. Posted November 26, 2022 Report Share Posted November 26, 2022 (edited) I have heard some things about thier stains that where not great. I have used a few of their materials over the decades with good results. They are selling tin at 30$ a pound it looks. A quik goggle search shows Shefeild pottery at 46$ a #.They are always top notch with stuff. I posted tin's huge price increase earlier this year here as well My guess is US Pigments has old stock left I know Laguna Clay Company went thru the roof earlier this year on Tin price You could order some and test it and let us know the outcomes? Edited November 26, 2022 by Mark C. Quote Link to comment Share on other sites More sharing options...
Stumonster Clayworks Posted November 26, 2022 Author Report Share Posted November 26, 2022 I ordered a #, will let you know in few weeks. Stuart Quote Link to comment Share on other sites More sharing options...
Hulk Posted November 26, 2022 Report Share Posted November 26, 2022 Hi Stuart, The only tin oxide I've used is from US Pigment - seems to work ok. I needed it for tin/chrome red (same recipe as Britt's "Chrome Red"). It's red! Pres 1 Quote Link to comment Share on other sites More sharing options...
Stumonster Clayworks Posted November 26, 2022 Author Report Share Posted November 26, 2022 @Hulk Thanks. I am going to try it on a white cone 6 oxidation - Lumos. I have made the Lumos before and the layering properties are amazing. Hulk and Pres 2 Quote Link to comment Share on other sites More sharing options...
fergusonjeff Posted November 28, 2022 Report Share Posted November 28, 2022 I also get my Tin from them and it has always been fine. Pres 1 Quote Link to comment Share on other sites More sharing options...