Nicky S Posted December 23, 2021 Report Share Posted December 23, 2021 I was able to find these programs So I think the earthenware is on a porcelain glaze firing ( which fires too1200 Right now it’s at 1029 degs Should I just switch off and pray to the kiln gods Any suggestions ASAP would really b appreciated Thank you Nicky Link to comment Share on other sites More sharing options...
Min Posted December 23, 2021 Report Share Posted December 23, 2021 If the clay you are firing is earthenware and the kiln is at 1029C and you want to follow the "Second Program" schedule you posted then I would quickly stop the kiln and restart it with the "Second Program" so you can get the 30 minute soak in. "Fourth Program" looks more like a midrange (cone 6-7) schedule. Link to comment Share on other sites More sharing options...
Nicky S Posted December 23, 2021 Author Report Share Posted December 23, 2021 10 minutes ago, Min said: If the clay you are firing is earthenware and the kiln is at 1029C and you want to follow the "Second Program" schedule you posted then I would quickly stop the kiln and restart it with the "Second Program" so you can get the 30 minute soak in. "Fourth Program" looks more like a midrange (cone 6-7) schedule. Thank you Min …. I left a few minutes more then switched off …. Got cold feet Hope I save something at least Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.